VascoMax® C-250 (UNS K92890)

Composition
Compound Al C Co Mn Mo
nominal wt. % 0.1 0.02 7.8 0.05 4.8
Compound Ni P S Si Ti
nominal wt. % 18.0 0.005 0.005 0.05 0.4

Mechanical Properties
Density lb/in3 (g/cm3)
0.289 (8.00)
Metallurgical Condition 1,500°F + age
Tensile Strength, ksi (MPa) 255 (1,759)
0.2% Yield Strength, ksi (MPa) 245 (1,690)
Elongation, % 12
Reduction in Area, % 50
Typical Hardness 48 HRC

VascoMax C-Series Technical Data Sheet 
in HTML or  PDF Format
Typical room temperature mechanical properties.

The information, data, and specifications presented here are representative only, and are not guaranteed values. Material or product applications described herein are solely for illustrative purposes and should not be construed as express or limited warranties for fitness for these or other applications.

Data are typical and should not be construed as maximum or minimum values for specification or for final design. Data on any particular piece of material may vary from those shown herein.