Search: 


Specialty Steel

ATI H-46

ATI 9-4-30

VascoMax® C-250

VascoMax C-300

VascoMax C-350

ATI 23

ATI AL 6XN®

ATI S240®

ATI 13-8Mo

ATI 13-8 SuperTough®

ATI 15-5

ATI 17-4 PH

ATI XM-19

ATI 304 L

ATI 316 L

ATI Datalloy 2® ESR

ATI Staballoy AG17™

REX 734™

ATI 455

ATI Jethete® M152

ATI A-286

ATI StabAlloy AG17™ (Unassigned)

Composition
Compound C Si Mn Cr N2 Mo
nominal wt. % 0.03 0.30 20.0 17.0 0.50 0.05

Mechanical Properties
Density lb/in3

0.284

 
Magnetic permeability1.005 max
Tensile Strength, ksi 150
0.2% Yield Strength, ksi 140
Elongation, %18%
Reduction in Area, %40%
Typical Hardness321 HB

ATI Staballoy AG17™ Technical Data Sheet 
in PDF Format

Typical room temperature mechanical properties.

The information, data, and specifications presented here are representative only, and are not guaranteed values. Material or product applications described herein are solely for illustrative purposes and should not be construed as express or limited warranties for fitness for these or other applications.

Data are typical and should not be construed as maximum or minimum values for specification or for final design. Data on any particular piece of material may vary from those shown herein.


Products | About Us | Careers | Contact