Composition
Compound C Si Mn Cr Mo Ni N
nominal wt. % 0.03 0.30 15.1 15.3 2.1 2.3 0.4

Mechanical Properties - Standard Properties
Density lb/in3 0.284
Magnetic Permeability1.005 max
Tensile Strength, ksi 155
0.2% Yield Strength, ksi 140
Elongation, %20
Reduction in Area, %50
Typical Hardness358 HB

ATI Datalloy 2® ESR 
in PDF Format

Typical room temperature mechanical properties.

The information, data, and specifications presented here are representative only, and are not guaranteed values. Material or product applications described herein are solely for illustrative purposes and should not be construed as express or limited warranties for fitness for these or other applications.

Data are typical and should not be construed as maximum or minimum values for specification or for final design. Data on any particular piece of material may vary from those shown herein.