Search: 


Titanium

ATI 30, Ti CP-1

ATI 40, Ti CP-2

ATI 55, Ti CP-3

ATI 70, Ti CP-4

ATI Grade 7

ATI Grade 12

ATI 3-2.5

ATI 6-4

ATI 6-4ELI

ATI 8-1-1

ATI 6-7

ATI 6-6-2

ATI 6-2-4-2

ATI 6-2-4-2-Si

ATI Ti-15Mo

ATI 6-2-4-6

ATI Ti-17

Stryker® TMZF®

ATI 15-3-3-3

ATI 38-644™

ATI TiOsteum®

ATI Grade 7 (UNS-R52400)

Nominal Composition - wt. %
C Fe H N O Pd Ti
0.10 max 0.30 max 0.015 max 0.03 max 0.25 max 0.12 - 0.25 rem

Mechanical Properties
Density lb/in3 (g/cm3) 0.163 (4.51)
Metallurgical Condition 1,300 °F anneal
Tensile Strength, ksi (MPa) 50 (345)
0.2% Yield Strength, ksi (MPa) 40 (276)
Elongation, % 20
Reduction in Area, % 25
Typical Hardness 80 HRB

Typical room temperature mechanical properties.

The information, data, and specifications presented here are representative only, and are not guaranteed values. Material or product applications described herein are solely for illustrative purposes and should not be construed as express or limited warranties for fitness for these or other applications.

Data are typical and should not be construed as maximum or minimum values for specification or for final design. Data on any particular piece of material may vary from those shown herein.